Cause

  • Restraint to slab movements induces cracks.
  • Cold joints
  • Deflection
  • High silt in concrete
  • Improper protection and curing
  • Early use

REMEDY IN BRIEF

  • Crack width ≥ 0.8mm
  • Pouring high bond strength flowable grout
  • Crack width 0.8 to 1.2 mm- Low viscosity resin based grout
  • Crack width ≤ 1.2mm- opening in strip for, Low viscosity resin based grout, stitching and patching the strip with high strength thin screed system.

Products